In the process of extracting lithium from sulfuric acid ore, the ore generally undergoes grinding, transformation roasting, acidification, leaching, purification, filtration and other processes to obtain a relatively pure lithium sulfate dilute solution.

White crystalline powder. Soluble in water, slightly soluble in alcohol. Can absorb carbon dioxide from the air and deterioration. It is strongly alkaline. It will not burn, but it is highly corrosive.

The ternary material and the precursor are loose powder, but the fluidity is not good. According to the production process, the ratio and the particle size are different, the water content before drying is generally about 10% ~ 20%, and the water content of the product after drying is about 0.2.

Mesophase carbon microbeads are micron-sized spherical carbon materials formed by thermal condensation polymerization of asphalt compounds during heat treatment to generate anisotropic mesophase small spheres and separated from the asphalt matrix.